| Mechanical Properties |
| Ultimate tensile strength |
890 – 1200 MPa |
| Yield strength |
590 – 890 MPa |
| Young’s modulus (modulus of elasticity) |
190 – 196 GPa |
| Elongation at break |
7 – 16 % |
| Physical Properties |
| Corrosion resistance |
Good |
| Magnetism |
Magnetic |
| Weldability |
Good |
| Thermal Properties |
| Maximum service temperature |
820 °C |
| Thermal expansion coefficient |
10.4 – 11.7 × 10-6/ºC |
| Thermal conductivity |
17 – 22 W/(m⋅°C) |
| Electrical Properties |
| Electrical resistivity |
77 μΩ*cm |
| Post Treatments |
| Post-Processing |
Hot working, Age hardening, Annealing |
| Anodizing compatibility |
Not suitable |
| Common Applications |
| High pressure corrosive environments |
Gears & Fasteners |
| Fittings & shafts in aircraft components |
Chemical process equipment |
| Equipment for nuclear reactors |
|