Delrin (POM) vs Nylon for Machined Plastic Parts

Inhaltsübersicht

Startseite - Blogs - Blogs - Delrin (POM) vs Nylon for Machined Plastic Parts
Nylon printed gear and machined component

Delrin (POM) vs Nylon for Machined Plastic Parts

Delrin vs nylon is a choice between acetal homopolymer and a specified polyamide grade for a working component. Start with moisture exposure, sliding contact, stiffness and the fit to the mating part. MXY’s Standard plastic machining tolerance is ±0.25 mm (±0.010 in). A bushing, locating nest and flexible latch need different material evidence.

How should a Delrin vs nylon comparison start?

Design questionDelrin and other acetal stockNylon stock
What exactly is being bought?Identify Delrin acetal homopolymer or the particular POM stock grade offeredIdentify the polyamide, its exact stock grade and any reinforcement
What affects a close fit?Check stock condition, clamping, service temperature and final inspection stateAlso define the moisture condition represented by the material and inspection
Where does sliding take place?Identify the mating material, contact pressure, speed and lubricationIdentify the same conditions and the exposure or conditioning affecting the running fit
What should the first article show?Accepted bore or locating feature in its defined stateAccepted feature in the specified condition and fit to the representative assembly

Acetal is often called POM. Delrin is a trade name for acetal homopolymer, while acetal copolymer is another material within the POM family. A drawing that intends a specific product should name it. If an equivalent grade can be proposed, give the engineer a route to judge it against the required properties, stock form and performance in the actual assembly. Do not assume that a quote for unspecified acetal represents the originally tested material.

Nylon covers a group of polyamides, including PA6, PA66 and PA12. The unfilled bar stock used for a machined guide can differ from a reinforced molding resin or powder-bed material with the same broad family name. Identify the stock the machinist will cut. For a grade or production-route comparison, the polyamide and nylon material guide explains how the process and grade enter the purchase requirement.

Tolerances depend on part size, geometry and material; each Precision or Best tolerance is confirmed feature-by-feature on the quotation together with the inspection method. Review the POM and Delrin material options, then include the grade and drawing in the quotation request. The manufacturing guides cover related process decisions.

How does moisture affect the fit of a machined part?

Nylon can take up moisture from its surroundings. The resulting material condition affects dimensions and mechanical behavior. Acetal generally absorbs less moisture, which can make it a useful starting point when a locating feature must hold a repeatable fit in changing humidity. The selection still depends on the specific grade, part geometry, load, temperature and accurate representation of the environment on the drawing.

Imagine a bushing measured dry after machining, then installed in equipment that receives regular washdown. The inspection record should identify what condition it describes. A loose bushing in a measuring room does not necessarily represent the final condition of the part installed in a metal housing and exposed in use. If the running fit is critical, establish with the design engineer when the part is measured and how it is conditioned before the assembly check.

Read moisture data with its test method and condition. Equilibrium in a stated atmosphere, absorption after immersion and a brief exposure interval are different measurements. The part drawing should say which condition matters to the project. When a procurement specification sets a particular moisture requirement, use the material maker's data for the actual stock offered and retain the measurement condition along with the result. A family-wide percentage cannot establish the finished bore clearance.

Beige polymer plate with a central groove and mounting holes

Which material should I consider for a bushing or wear strip?

Identify the contact pair first. A machined polymer running on a polished steel shaft behaves differently from a guide sliding against containers, a plated rail or another polymer. Give the mating material, finish, movement, contact load and any lubrication. Specify whether the component moves continuously, oscillates through a short travel or only moves during installation. These conditions determine which wear or friction evidence is useful.

For a flanged bushing, the outside diameter fixes the part in its housing and the inside diameter controls clearance to the shaft. Pressing the bushing into a housing can change the bore. Record the housing geometry, the axial seating face and whether final acceptance takes place loose or installed. A candidate material that appears to fit in an isolated loose sample may show different running clearance once restrained in its working housing.

For a wear strip, the support underneath the working face can matter more than the nominal thickness of an unsupported sample. Show where the strip is fastened and where movement along its length is permitted. If the assembly uses slots, distinguish the location that establishes position from the slots that allow movement. A long flexible strip and a short rigid bushing need different workholding and different inspection evidence even when both are made from the same grade.

How do machining and workholding affect dimensional stability?

Stock condition, material removal, temperature and clamping all influence the geometry measured after machining. A thick sheet machined deeply on one side can move when held material is removed. Mark which surface establishes the working reference and which faces are available for clamping. If a thin wall is measured while the part is still constrained, identify the independent check that represents the released component.

MXY’s Standard plastic tier is ±0.25 mm (±0.010 in), and the Precision tier is ±0.05 mm (±0.002 in) for features marked critical on the drawing. Assign the closer requirement to the feature that actually locates a component or controls working clearance. A tight bore size does not control where its axis lies relative to a mounting face. Put that relationship directly on the drawing and define the condition of the finished part during inspection.

Consider a fixture nest with pads that support a metal workpiece and a pocket that clears a protruding screw. The pad positions and the fit of a locating pin determine repeatability. The clearance pocket can have more freedom provided the workpiece can be loaded. Mark those roles so the machinist can plan clamping and inspection around the actual contacts. A close limit on the outside contour adds little if the fixture is located from internal features.

How should the buyer compare friction and wear evidence?

The relevant result belongs to a material pair and a set of conditions. A coefficient from a grade sheet may describe a test against a particular opposing material and surface under a specified load and motion. Compare those conditions with the application. A sliding guide that is washed and left dry has a different test context from a lubricated shaft rotating in a closed housing.

Give the supplier any wear limit that changes the product's function. A guide may tolerate a polished contact track as long as alignment stays within the drawing. A bushing might require the shaft to stay within a permitted range after movement. A gear can need both a fit check at its bore and an assessment of its working tooth surfaces. Describe the observation and the required result instead of asking for a universally low-friction material.

If a reinforced nylon is proposed, include the mating surface in the comparison. Reinforcement can change contact behavior as well as stiffness. A small coupon can support an early screening comparison, but a trial with the intended contact geometry, support, motion and material condition gives the engineer evidence closer to the released component. Keep the coupon and component results separate in the project record.

White machined polymer rectangular frame with mounting holes

How to specify it on your drawing

  • Name the exact acetal or polyamide grade, stock form, supplied condition and any approved alternatives.
  • Mark the surface that locates the part in the assembly, the mating material and the working direction of motion.
  • Identify critical sizes or geometric relationships, the inspection condition and whether the part is loose or installed.
  • Describe the environment, moisture condition, temperature, cleaning exposure and any required lubrication.
  • Specify the final surface condition, edge treatment and any requirement for a material certificate or functional sample.

How MXY produces machined acetal and nylon components

MXY engineers review the released model and drawing for tool access, holding and inspection. Standard plastic dimensions are ±0.25 mm (±0.010 in), and Precision on critical plastic features is ±0.05 mm (±0.002 in). CNC prototypes take 3–7 business days and production takes 10–15 business days from order confirmation, shipping excluded. Quotes within 24 hours; CNC, sheet metal and 3D printing usually within 12 hours, with DFM feedback included. Identify the required stock grade and working fits for custom CNC machining.

FAQ

Is Delrin another name for every acetal grade?

Delrin identifies acetal homopolymer products. A supplier can also offer other POM grades, including acetal copolymer. Specify the tested grade or define what an alternative must demonstrate before it is accepted for the part.

Is nylon appropriate for a close-fitting bore?

Review the grade, moisture condition, temperature, housing restraint and the permitted installed clearance. Specify how and when the bore is checked. If a close fit governs material choice, compare samples under the same conditions as the intended assembly.

Which should I use for a part that slides without lubrication?

Describe the mating surface, load, travel and operating environment. Review grade-specific evidence under comparable conditions and test a representative component. The family name alone cannot establish wear life or working clearance in the particular motion.

How should I compare a sample made from a different stock shape?

Record the original and proposed grade, supplied condition, form, release revision and machining sequence. Identify features controlled in the free or assembled state. Recheck the working surfaces against the same mating components and inspection reference.

Which parts of a fixture usually need the closest control?

Identify the contacts that actually locate the workpiece or establish its height and orientation. Give those features individual requirements when the general tolerance is insufficient. A nearby opening used only for tool or fastener access can often be defined by its clearance function.

Nehmen Sie Kontakt mit CNC-Bearbeitungsdienstleistern auf

Werden Sie unser Partner für maßgeschneiderte CNC-Teile

Kontakt aufnehmen

STEP-Modell und PDF-Zeichnung gemeinsam auswählen. Vor dem Hochladen vertraulicher Zeichnungen bitte eine Vertraulichkeitsvereinbarung anfordern.

STEP, IGES, X_T, SLDPRT or STL plus PDF drawing, up to 100 MB.

Verwandte Artikel und Einblicke