| Property | Value |
|---|---|
| Mechanical Properties | |
| Ultimate tensile strength | 25 – 31 MPa |
| Yield strength | 14 – 41.4 MPa |
| Young’s modulus (modulus of elasticity) | 0.39 – 2.25 GPa |
| Elongation at break | 300 – 450 % |
| Hardness | 50 – 65 Shore D |
| Physical Properties | |
| UV resistance | Good |
| Thermal Properties | |
| Maximum service temperature | 250 – 270 °C |
| Thermal expansion coefficient | 7 – 20 × 10-6/ºC |
| Thermal conductivity | 0.23 – 0.5 W/(m⋅°C) |
| Electrical Properties | |
| ESD Safety | No |
| Common Applications | |
| Chemical engineering | General machinery construction |
| Electrical applications | Food industry |