{"id":1468,"date":"2025-01-31T04:36:11","date_gmt":"2025-01-31T04:36:11","guid":{"rendered":"https:\/\/cnc-machiningservices.com\/?post_type=material&#038;p=1468"},"modified":"2025-04-28T17:28:56","modified_gmt":"2025-04-28T17:28:56","slug":"titan-grad-1-3-7025","status":"publish","type":"material","link":"https:\/\/cnc-machiningservices.com\/de\/material\/titan-grad-1-3-7025\/","title":{"rendered":"Titan Grad 1 | 3.7025"},"content":{"rendered":"<!DOCTYPE html>\n<html lang=\"en\">\n<head>\n    <meta charset=\"UTF-8\">\n    <meta name=\"viewport\" content=\"width=device-width, initial-scale=1.0\">\n    <style>\n        table {\n            width: 100%;\n            border-collapse: collapse;\n            font-size: 14px; \/* Default WordPress font size *\/\n        }\n        th, td {\n            border: 1px solid black;\n            padding: 8px;\n            text-align: left;\n        }\n        th {\n            font-weight: bold;\n        }\n        td:first-child {\n            width: 50%;\n        }\n        td:last-child {\n            width: 50%;\n        }\n    <\/style>\n<\/head>\n<body>\n\n<table>\n    <thead>\n        <tr>\n            <th>Eigentum<\/th>\n            <th>Wert<\/th>\n        <\/tr>\n    <\/thead>\n    <tbody>\n        <tr>\n            <td colspan=\"2\"><strong>Mechanische Eigenschaften<\/strong><\/td>\n        <\/tr>\n        <tr>\n            <td>H\u00f6chste Zugfestigkeit<\/td>\n            <td>310 - 350 MPa<\/td>\n        <\/tr>\n        <tr>\n            <td>Streckgrenze<\/td>\n            <td>220 - 240 MPa<\/td>\n        <\/tr>\n        <tr>\n            <td>E-Modul (Elastizit\u00e4tsmodul)<\/td>\n            <td>103 - 105 GPa<\/td>\n        <\/tr>\n        <tr>\n            <td>Dehnung bei Bruch<\/td>\n            <td>28 &#8211; 32 %<\/td>\n        <\/tr>\n        <tr>\n            <td>H\u00e4rte<\/td>\n            <td>120 HB<\/td>\n        <\/tr>\n\n        <tr>\n            <td colspan=\"2\"><strong>Physikalische Eigenschaften<\/strong><\/td>\n        <\/tr>\n        <tr>\n            <td>Korrosionsbest\u00e4ndigkeit<\/td>\n            <td>Ausgezeichnet<\/td>\n        <\/tr>\n        <tr>\n            <td>Magnetismus<\/td>\n            <td>Nicht-magnetisch<\/td>\n        <\/tr>\n        <tr>\n            <td>Schwei\u00dfeignung<\/td>\n            <td>Hoch<\/td>\n        <\/tr>\n\n        <tr>\n            <td colspan=\"2\"><strong>Thermische Eigenschaften<\/strong><\/td>\n        <\/tr>\n        <tr>\n            <td>Maximale Betriebstemperatur<\/td>\n            <td>320 - 400 \u00b0C<\/td>\n        <\/tr>\n        <tr>\n            <td>W\u00e4rmeausdehnungskoeffizient<\/td>\n            <td>8.35 - 8.6 \u00d7 10<sup>-6<\/sup>\/\u00baC<\/td>\n        <\/tr>\n        <tr>\n            <td>W\u00e4rmeleitf\u00e4higkeit<\/td>\n            <td>16 - 21 W\/(m\u22c5\u00b0C)<\/td>\n        <\/tr>\n\n        <tr>\n            <td colspan=\"2\"><strong>Elektrische Eigenschaften<\/strong><\/td>\n        <\/tr>\n        <tr>\n            <td>Elektrischer Widerstand<\/td>\n            <td>42 - 45 \u03bc\u03a9*cm<\/td>\n        <\/tr>\n\n        <tr>\n            <td colspan=\"2\"><strong>Post-Behandlungen<\/strong><\/td>\n        <\/tr>\n        <tr>\n            <td>Nachbearbeitung<\/td>\n            <td>Kalt- und Warmumformung, Gl\u00fchen. Nicht h\u00e4rtbar durch W\u00e4rmebehandlung.<\/td>\n        <\/tr>\n        <tr>\n            <td>Kompatibilit\u00e4t mit Eloxal<\/td>\n            <td>Geeignet<\/td>\n        <\/tr>\n\n        <tr>\n            <td colspan=\"2\"><strong>Gemeinsame Anwendungen<\/strong><\/td>\n        <\/tr>\n        <tr>\n            <td>Komponenten der Flugzeugzelle<\/td>\n            <td>Kryogenische Beh\u00e4lter<\/td>\n        <\/tr>\n        <tr>\n            <td>W\u00e4rmetauscher<\/td>\n            <td>CPI-Ausr\u00fcstung<\/td>\n        <\/tr>\n        <tr>\n            <td>Verfl\u00fcssiger-Rohrleitungen<\/td>\n            <td>Einlegek\u00f6rbe<\/td>\n        <\/tr>\n    <\/tbody>\n<\/table>\n\n<\/body>\n<\/html>","protected":false},"excerpt":{"rendered":"<p>Property Value Mechanical Properties Ultimate tensile strength 310 &#8211; 350 MPa Yield strength 220 &#8211; 240 MPa Young&#8217;s modulus (modulus of elasticity) 103 &#8211; 105 GPa Elongation at break 28 &#8211; 32 % Hardness 120 HB Physical Properties Corrosion resistance Excellent Magnetism Non-magnetic Weldability High Thermal Properties Maximum service temperature 320 &#8211; 400 \u00b0C Thermal [&hellip;]<\/p>","protected":false},"featured_media":0,"parent":0,"template":"","format":"standard","meta":{"_acf_changed":false,"footnotes":""},"material-category":[33,53],"class_list":["post-1468","material","type-material","status-publish","format-standard","hentry","material-category-cnc-machining-metals","material-category-titanium"],"acf":[],"_links":{"self":[{"href":"https:\/\/cnc-machiningservices.com\/de\/wp-json\/wp\/v2\/material\/1468","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/cnc-machiningservices.com\/de\/wp-json\/wp\/v2\/material"}],"about":[{"href":"https:\/\/cnc-machiningservices.com\/de\/wp-json\/wp\/v2\/types\/material"}],"version-history":[{"count":2,"href":"https:\/\/cnc-machiningservices.com\/de\/wp-json\/wp\/v2\/material\/1468\/revisions"}],"predecessor-version":[{"id":4893,"href":"https:\/\/cnc-machiningservices.com\/de\/wp-json\/wp\/v2\/material\/1468\/revisions\/4893"}],"wp:attachment":[{"href":"https:\/\/cnc-machiningservices.com\/de\/wp-json\/wp\/v2\/media?parent=1468"}],"wp:term":[{"taxonomy":"material-category","embeddable":true,"href":"https:\/\/cnc-machiningservices.com\/de\/wp-json\/wp\/v2\/material-category?post=1468"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}